Equivalent designations
UNS N10675
DIN W. Nr. 2.4600
Form |
ASTM |
Rod |
B 335 |
Plate, sheet and strip |
B 333, B 906 |
Seamless pipe and tube |
B 622 |
Welded pipe |
B 619, B 775 |
Welded tube |
B 626, B 751 |
Welding fitting |
B 366 |
Forged or rolled pipe flange and forged fitting |
B 462 |
Billet and bar for reforging |
B 472 |
Forging |
B 564 |
Chemical composition
% |
Ni |
Mo |
Ni+Mo |
Cr |
Fe |
W |
Co |
C |
Mn |
Si |
P |
S |
Al |
Ti |
Cu |
Nb |
Ta |
V |
Zr |
min |
65.0 |
27.0 |
94.0 |
1.0 |
1.0 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
max |
|
32.0 |
98.0 |
3.0 |
3.0 |
3.0 |
3.0 |
0.010 |
3.0 |
0.10 |
0.030 |
0.010 |
0.50 |
0.20 |
0.20 |
0.20 |
0.20 |
0.20 |
0.10 |
Physical properties
Density |
9.22 g/cm3 |
Melting range |
1370-1418℃ |
Features: Hastelloy B-3 has outstanding resistance to hydrochloric acid at all concentrations and temperatures. It also resists sulfuric, phosphoric, formic, acetic acids and other nonoxidizing media. It has excellent resistance to pitting corrosion, stress corrosion cracking, and knife line and weld heat-affected zone attack. Hastelloy B-3 has greater thermal stability than Hastelloy B-2.
Applications: Hastelloy B-3 is suitable for the applications where Hastelloy B-2 is required. Like Hastelloy B-2, Hastelloy B-3 should not be used in the presence of ferric or cupric salts as these salts may cause rapid corrosion attack.