Standard Grade |
Trade Name |
UNS No. |
DIN |
BS |
JIS |
French Specs |
Hastelloy C-22 |
UNS N06022 |
WS 2.4602 |
- |
- |
- |
|
Specification |
ASTM B 622/B 829 & ASME SB 622/SB 829 |
|||||
Typical use
|
C- 22 (UNS N06022) is the most versatile Nickel-Chromium-Molybdenum-Tungsten alloy with controlled Iron. Due to Alloy 22's content this alloy exhibits excellent resistance to both oxidising and reducing acid environments as well as those containing mixed acids. Alloy C- 22 is particularly useful for resistance to pitting and crevice corrosion in acid-halide environments. Alloy C-22 is used in pickling chlorination, sulphonation plants, pollution control, chemical processing, marine and nuclear fuel reprocessing. |
|||||
Weight Formula |
Average Wall: (OD-WT) x WT x 0,0271 = Kg/m (all sizes in mm) |
Chemical Composition Limits |
||||||||||||
Weight % |
Ni |
Cr |
Mo |
Fe |
W |
Co |
V |
C |
Mn |
S |
Si |
P |
C- 22 (N06022) |
Bal |
20-22 |
12.5-14.5 |
2-6 |
2.5-3.5 |
2.5 max |
0.35 max |
0.015 max |
0.50 max |
0.02 max |
0.08 max |
0.02 max |
Material |
Tensile Strength MPa |
Yield Strength (0.2% Offset) |
Elongation |
Hardness |
||
ksi |
MPa |
ksi |
MPa |
% |
Rockwell |
|
C- 22 (N06022) |
100 |
690 |
45 |
310 |
45 |
- |